Home / Services / Stainless & aluminum

Stainless & aluminum

Stainless and aluminum welding with TIG precision, on-site

Stainless and aluminum do not forgive shortcuts. Our stainless and aluminum welding service uses TIG and careful heat control to repair and fabricate food equipment, handrails, tanks, boat parts, ladders and toolboxes where they are installed, with filler, gas and cleanup matched to the alloy.

Welder operating a welding machine in a shop

Quick answer

Stainless and aluminum welding is precision work, usually done with TIG, on metals that react badly to excess heat and contamination. A mobile welder repairs stainless food equipment, rails and tanks with matched filler and back-purging, and welds aluminum boat parts, ladders, trailers and toolboxes after removing oxide, then cleans the work so it resists corrosion.

Key points

TIG welding for stainless steel and aluminum in thin and medium gauges

Food and beverage equipment, sinks, tables, rails and tanks repaired in place

Aluminum boat parts, ladders, toolboxes, ramps and trailer components

Filler alloys, shielding gas and back-purging matched to the job

Heat tint removal and passivation guidance so stainless stays stainless

Why stainless and aluminum need a different approach

Carbon steel tolerates a lot. Stainless and aluminum do not. Stainless can lose its corrosion resistance if overheated or contaminated with carbon steel particles, and it distorts easily on thin sheet. Aluminum conducts heat away so fast that the puddle behaves completely differently, and it is covered by a tough oxide layer that melts at a far higher temperature than the metal underneath.

That is why this work is done with TIG in most cases. TIG gives precise control over heat input and filler, produces clean welds with no spatter, and handles thin material that would burn through with wire processes. For thicker aluminum on trailers and boat structures, a spool gun MIG setup is sometimes faster and equally sound.

Stainless steel: food equipment, rails and tanks

Most stainless we weld is 304 or 316. Type 304 is common in kitchens, food service and indoor rails; 316 contains molybdenum for better resistance to chlorides and is the usual choice near salt water or chemicals. Filler is matched accordingly, typically 308L for 304 and 316L for 316, with low carbon to help preserve corrosion resistance.

Where the back side of a weld will be exposed, as inside a tank or a sanitary tube, the back is purged with argon so it does not oxidize into a rough, corrosion-prone surface. Afterward, heat tint is removed and the surface is cleaned so the protective layer can reform. Typical jobs include cracked prep tables, sink and drainboard seams, brackets on food trucks, handrail joints, brewery platform parts and small tank fittings.

Metalworker holding a tool in a workshop

Aluminum: boats, ladders, trailers and toolboxes

Aluminum work around Houston leans heavily marine: pontoon brackets, T-tops, ladders, rub rails, jon boat seams and trailer bunks, all of which live in humid and often salty conditions. Truck toolboxes, ramps, diamond plate and access ladders round out the list.

Each joint is cleaned with a stainless brush and solvent to remove oxide and oils, then welded with AC TIG or a spool gun. Filler choice matters: 4043 flows well and resists cracking on many 6xxx alloys, while 5356 is stronger and better matched to marine 5xxx alloys and parts that will be anodized. Heat-treated alloys like 6061-T6 lose a meaningful part of their strength near the weld, so we reinforce structural repairs or replace sections where needed.

Food trucks combine both metals in one small, hard-working space: stainless counters and hood brackets on an aluminum or steel body, all bouncing down the road every day. Cracked mounts and broken seams on those units can usually be handled in a single visit wherever the truck is parked, which matters when every day off the street is lost revenue. That holds for operators parked around Houston and in suburbs like Sugar Land.

Galvanic corrosion: when stainless, aluminum and steel meet

Different metals in contact, plus moisture, form a small battery. The less noble metal corrodes faster, and in salty or humid air the effect can eat through aluminum surprisingly quickly. It is one of the most common reasons for repeat failures we see on boats, trailers and coastal railings.

When we repair a joint, we look at the fasteners and contact points around it. Steel bolts in aluminum ladders, carbon steel brackets on stainless rails and aluminum fittings resting on galvanized steel all need attention.

Use stainless fasteners with isolating washers on aluminum where possible

Separate dissimilar metals with nylon, neoprene or barrier tape

Never wire-brush stainless with a brush used on carbon steel

Rinse salt deposits off marine aluminum and stainless regularly

Thin gauge welding without warping or burn-through

Thin stainless sheet on a prep table or aluminum diamond plate on a toolbox can warp badly if welded too hot or too fast in one area. We manage that with tight fit-up, small tacks spaced evenly, short welds sequenced around the part, copper or aluminum backing bars to pull heat away, and pulsed TIG where it helps.

Cosmetic work gets extra care. On visible stainless, such as handrails or front-of-house equipment, welds can be blended and refinished to closely match the surrounding brushed grain, so the repair is hard to spot.

How a stainless & aluminum job works with Houston Mobile Welding

01

Identify the metal and use

Send photos, any stamps or part numbers, and what the part does, such as food contact, marine use or structural load.

02

Plan filler, gas and finish

The written quote specifies the process, filler alloy, purge needs, cosmetic finish and any parts to replace.

03

Clean, fit and TIG weld

Joints are cleaned of oxide and oils, fit tightly, and welded with controlled heat to limit distortion.

04

Clean up and protect

Heat tint is removed from stainless, aluminum is cleaned, and we review galvanic issues and upkeep with you.

Stainless or aluminum? Identifying the metal first

Plenty of parts arrive described as stainless when they are aluminum, or as aluminum when they are plated steel. Since filler and process depend on the alloy, identification comes before any welding. A few quick checks help, and photos with any part numbers or stamps help us even more.

If a part is a casting, carries a pressure rating, or is food-contact equipment with a manufacturer warranty, tell us in the request so we can advise whether welding is the right path.

A magnet: 300-series stainless is mostly non-magnetic, carbon steel is strongly magnetic

Weight: aluminum feels about a third as heavy as steel of the same size

Scratch: aluminum is soft and shows bright, dull-gray metal underneath

Rust: red rust usually means carbon steel or contamination on stainless

Preparing for repair, and what drives the cost

Empty and clean the part before the visit. Food equipment should be emptied, cleaned and sanitized, and tanks must be drained and free of fuel, chemicals or vapor before any welding, which may require professional cleaning first. Boats should be on a trailer or lift with the repair area dry.

Price depends on access, thickness, joint length, whether back-purging is needed, and how much cosmetic finishing the part requires. Aluminum trailer frames often overlap with our trailer and truck repair work, and stainless plant fixtures with pipe and industrial welding. Aluminum gates and railings fall under gates and security bars.

Frequently asked questions

Can you weld stainless food equipment on-site?

Yes. Prep tables, sinks, drainboards, shelving, hood brackets and food truck fixtures are common jobs. Equipment must be emptied, cleaned and powered down before we arrive. We TIG weld with low-carbon filler matched to the stainless grade, remove heat tint afterward and blend the finish where appearance matters, so the surface stays cleanable and corrosion resistant.

What filler do you use on aluminum?

It depends on the alloy and the part. 4043 is common for many 6xxx alloys because it flows well and resists cracking. 5356 is stronger and better suited to marine 5xxx alloys and parts that will be anodized. We match filler to the base metal and the job, and identify the alloy first when it is unknown.

Why did my aluminum ladder or boat bracket corrode so fast?

Galvanic corrosion is a frequent cause. When aluminum touches steel or stainless in the presence of salt or moisture, the aluminum corrodes faster. Steel bolts, galvanized brackets and stainless hardware without isolation are common triggers. We repair the damage and recommend fastener and isolation changes so the problem does not come right back.

Can you weld a fuel or chemical tank?

Only after it has been drained and made free of flammable or hazardous vapors, which often requires professional cleaning and gas testing. Welding a tank that has held fuel without proper cleaning is extremely dangerous. If you have a tank repair, describe what it held in the request, and we will explain the cleaning steps needed before any welding can happen.

Will a stainless weld rust?

A properly made stainless weld, with matched filler, clean technique and heat tint removed, should resist corrosion much like the surrounding metal. Rust appears when stainless is contaminated with carbon steel particles, overheated, or left with heavy heat tint. We use dedicated stainless brushes and abrasives and clean the finished weld so its protective layer can reform.

Can you repair aluminum truck toolboxes and diamond plate?

Yes. Cracked toolbox seams, broken lid hinges, loose mounting brackets and torn diamond plate are routine TIG repairs. Thin diamond plate needs careful heat control to avoid warping. Toolboxes should be emptied before the visit. If the cracks keep returning at the mounting points, we may suggest added reinforcement or rubber isolators to reduce vibration.

Get stainless or aluminum repaired right

Send photos, any part markings and what the piece is used for. You will get a written quote with the process, filler and finish spelled out.

Get a Free Quote
Welder creating blue sparks during an on-site repair
Houston Mobile Welding logo

On-site welding repairs and fabrication anywhere in Houston.

Free written quote · No obligation · Reply within one business day

Houston Mobile Welding

Get a free quote

Tell us what you need built or repaired. We'll reply with a clear written quote.